CA180L ʻAno Huihui a me ka wai holoi non-phosphorus
Hōʻike huahana
1. Hiki i ka mea holoi holoi ke hoopuehu a holoi i ka popo lepo ma ka paia o ka punawai, e hoonui loa i ka pono o ka neenee a hoonui i ka cementaƟ ma ka mana ma waena o ka sima a me ka paia.
2.E hoʻohana ma lalo o ka mahana o 180 ℃ (356 ℉, BHCT).
ʻO 3.Compound holoi wai i hōʻike ʻia me ka non-phosphorus, non-toxic a me nā ʻano haʻahaʻa haʻahaʻa, i hoʻohana nui ʻia e like me ka holoi ʻana a me nā mea hoʻokaʻawale i ka wā o ke kaʻina o ka luawai aila cementing kahi e hoʻohana ʻia ai ka wai wili wai. Hiki ke hoʻokō ʻia ka hana maikaʻi ke hoʻohana ʻia i loko o ka wai wili ʻaila.
4. I ka hana ʻana i ka wai holoi hou ma o ka hoʻohana ʻana iā CW110L, pono e hana mua ʻia ka hoʻāʻo hoʻohālikelike.
5. ʻAʻole hiki ke hana i ka wai holoi ma ka hoʻohana ʻana iā CW110L me ka wai hui ʻana i loaʻa nā mea hoʻohui ʻē aʻe a i ʻole ka paʻakai kiʻekiʻe. A i ʻole hiki ke kū mai nā hopena maikaʻi ʻole ma muli o ka like ʻole.
6. ʻO ka mālama ʻana i ka wā lōʻihi e hopena i ka lepo a me ka blurry hiʻohiʻona o CA180L, he mea maʻamau a ʻaʻohe mana i kāna hana.
Nā kikoʻī
Ka nana aku | ʻO ka mānoanoa, g/cm3 | Wai-Solubility |
Wai wai ʻulaʻula | 1.40±0.05 | Hiki ke hoʻoheheʻe |
ʻO ka ʻōlelo kuhikuhi wai holoi
ʻO ka mānoanoa slurry sima | Manaʻo ʻia |
Ka wai hou | 600g |
CA180L wai holoi | ʻO ka maʻamau 2.0-6.0% (BWOW), ʻōlelo ʻia ʻo 4.0% (BWOW) |
Hana wai holoi
'ikamu | Kūlana hoʻāʻo | Hōʻike ʻenehana |
Holoi pono ma ka ili o ka paipu pahu (10min),% | ʻO ka wikiwiki o ka hoʻololi ʻana i ka viscometer me ka rotor crude-treated he 300r/min (e wehe i nā pahu o loko), ka wela wela≥38 ℃ | ≥60 |
Puke maʻamau a me ka waiho ʻana
1.Packed i 25kg, 200L a me 5 US galani pahu pahu. Loaʻa nō hoʻi nā pūʻolo i hana ʻia.
2.Customized pūʻolo pūʻolo. Ma hope o ka pau ʻana, e hoʻāʻo ʻia ma mua o ka hoʻohana ʻana.
Pūʻolo
25KG/BAG a i ʻole e like me kāu noi.
Waihona
E kūʻai ma kahi ea, maloʻo.
Kūlana hoʻokō
Kūlana International.